High energy storage properties of 0.94Bi<sub>0.5</sub>Na<sub>0.5</sub>TiO<sub>3</sub>-0.06BaTiO<sub>3</sub> ceramics by incorporating <InlineParagraph>Sr<sub>0.8</sub>Bi<sub>0.1γ0.1</sub>Ti<sub>0.8</sub>Zr<sub>0.2</sub>O<sub>2.95</sub></InlineParagraph>

Figure 3. Temperature-dependent dielectric permittivity and loss of (1-x)BNBT-xSBTZ ceramics from 70 to 400 °C at 1 kHz, 10 kHz, 1 MHz, 10 MHz, and 20 MHz, respectively. (A) x = 0.07, (B) x = 0.09, (C) x = 0.09, and (D) x = 0.10.